Skip to main content

🇻🇳 178 profiles · Engineering review

Vietnam Manufacturing

What Tolerance Grades Should I Know When Purchasing Stamping Parts?

July 17, 2026

CNC punching machine at Adong Interior And Advertising, a DEWIN-audited Vietnamese factory

Key tolerance grades to know when purchasing metal stamping parts

Tolerance grades for stamping parts confused one of our U.S. clients so much that they over-specified every feature on their bracket drawing — and their unit cost jumped 40%.

When purchasing stamping parts, you should know the ST1–ST11 flat grades and FT1–FT10 formed grades under GB/T13914, plus the globally used ISO 2768 classes (fine, medium, coarse, very coarse) and DIN 6930 grades (f, m, g, sg). Defaulting to ISO 2768-m or ST3–ST5 covers most industrial applications cost-effectively.

This guide breaks down every major tolerance grading system, explains which grades fit which features, and shows you how to avoid paying for precision you do not need. Let’s walk through each system step by step.

What Are the Standard Tolerance Grades Used in Metal Stamping and How Do They Affect My Sourcing Decisions?

A purchasing manager in Ohio once sent us a drawing with every dimension marked "Fine." When our engineering team in China reviewed it, we found that only three of the twenty-two dimensions actually needed that level of dimensional accuracy. The rest could safely sit at "Medium."

The standard tolerance grades used in metal stamping include GB/T13914's ST1–ST11 for flat parts and FT1–FT10 for formed parts, ISO 2768's four classes (f, m, c, v), and DIN 6930's four levels (f, m, g, sg). Your sourcing decisions depend on matching the right grade to each feature's function.

Standard tolerance grades GB/T13914, ISO 2768, and DIN 6930 for metal stamping

GB/T13914: The ST and FT System

If you source stamping parts from Asian suppliers, you will encounter GB/T13914-2002. This Chinese national standard splits tolerances into two categories based on part geometry.

Flat stamping parts use ST grades. These cover washers, flat brackets, shields, and any part with minimal bending. There are 11 grades, from ST1 (tightest) to ST11 (loosest). For most general industrial use, ST3 through ST5 is the sweet spot. ST1 and ST2 are rare and expensive.

Formed stamping parts use FT grades. These cover parts with bends, curls, or complex 3D shapes — like the Z-shaped spring clamps and multi-planar mounting brackets we regularly produce. There are 10 grades, from FT1 (tightest) to FT10 (loosest). FT grades are generally looser than ST grades for equivalent dimensions because material springback introduces process variation that is inherently harder to control.

Grade System Number of Grades Application Typical "Sweet Spot"
ST (Flat Stamping) 11 (ST1–ST11) Flat parts: washers, shields, flat brackets ST3–ST5
FT (Formed Stamping) 10 (FT1–FT10) Formed parts: bent brackets, clips, channels FT3–FT5
ISO 2768 1 4 (f, m, c, v) Global default for linear and angular dimensions Medium (m)
DIN 6930 4 (f, m, g, sg) European standard for stamped steel parts m (medium)

ISO 2768 and DIN 6930: The Global Standards

When our team works with European or American buyers, drawings almost always reference ISO 2768. It is the most ubiquitous standard for general sheet metal and machining tolerances worldwide. ISO 2768-m — the "Medium" class — is what most automotive structural parts 2 and non-critical features use. It covers linear dimensions, angular dimensions, and when paired with Part 2 (e.g., ISO 2768-K or ISO 2768-H), it also addresses geometrical tolerances like flatness and parallelism.

DIN 6930-2 is a German standard 3 built specifically for stamped steel parts. Its four accuracy levels — DIN 6930-f (fine), m (medium), g (coarse), and sg (very coarse) — specifically account for the physics of sheet metal forming. If you see DIN 6930-f on a drawing from a German OEM, that is the tightest class and will cost more.

The key takeaway for sourcing decisions: specify the grade that matches the feature's function. A bracket that holds a wire harness does not need the same precision as an electrical contact in a connector. Choosing the right grade saves money on tooling, inspection, and scrap.

✔ ISO 2768 Medium (m) is the industry default for most non-critical stamped features True
The vast majority of automotive and industrial stamping drawings specify ISO 2768-m as the general tolerance class because it balances cost with functional assembly requirements.
✘ All tolerance grades apply equally to flat and formed features False
Formed features inherently have wider tolerances than flat features because bending introduces material springback and process variation that cannot be eliminated entirely.
Video: Sample metal parts from audited Vietnamese factories in the DEWIN network. (@dewintech)

How Do I Know Which Tolerance Grade Is Right for My Custom Stamped Parts?

Last quarter, we ran a DFM review for a client whose bracket had twelve holes. Only two holes were alignment-critical. The rest were clearance holes for M4 screws. We recommended ±0.05 mm for the two critical holes and ±0.2 mm for everything else. That single change cut their die cost by roughly 15%.

The right tolerance grade depends on each feature's function. Use tighter grades (ST1–ST2, ISO 2768 Fine) only for mating surfaces, alignment holes, or electrical contacts. Use medium grades (ST3–ST5, ISO 2768-m) for general structural features. Use coarse grades for non-critical edges or rough stampings where dimensional accuracy has minimal impact on assembly.

Selecting the correct tolerance grade based on stamped part feature function

Match the Grade to the Feature Type

Not every dimension on a stamped part needs the same tolerance. Here is how our engineering team typically classifies features during a DFM review:

Pierced features (holes and slots): These are the easiest features to hold tight because the punch and die are rigid. On a progressive die, same-plane piercing can hold ±0.05 mm (±0.002"). Standard pierced holes typically fall in the ±0.10 mm to ±0.25 mm range. Hole-to-hole distances on the same station are extremely repeatable.

Formed heights and bends: These are harder to control. Material springback varies with sheet metal thickness, alloy type, and grain direction. Standard bend tolerances are ±0.2 mm to ±0.5 mm, with angular tolerances of roughly ±1 degree. Anisotropic compensation — adjusting the die angle to account for the metal's rolling grain direction — is how good toolmakers manage this.

Flatness: Large stamped panels can warp. Flatness is a geometrical tolerance that falls under Geometric Dimensioning and Tolerancing 4 (GD&T) principles or ISO 2768 Part 2. For parts under 25 mm (1 inch), expect about 0.13 mm (0.005") T.I.R. For larger parts, add roughly 0.1 mm per additional 25 mm of length.

Feature Type Standard Tolerance High Precision Tolerance Key Challenge
Pierced Holes / Slots ±0.10 mm to ±0.25 mm ±0.05 mm Tooling wear over time
Hole-to-Hole (Same Plane) ±0.13 mm (0.005") ±0.05 mm (0.002") Station alignment
Formed Heights / Bends ±0.2 mm to ±0.5 mm ±0.15 mm Material springback
Angular (Bends) ±1° ±0.5° Springback, grain direction
Flatness (0–25 mm span) 0.13 mm T.I.R. 0.08 mm T.I.R. Internal stress
Bend-to-Hole Distance ±0.38 mm (0.015") ±0.20 mm Bend line shift

Consider the Material

The alloy you choose directly impacts what tolerance grade is achievable. Harder materials resist clean shearing and introduce more springback. Our team in Vietnam has found this to be especially pronounced with stainless steel and high-strength alloys.

Material Piercing Tolerance Gauge Tolerance Notes
Mild Steel ±0.05 mm (±0.002") ±0.13 mm (±0.005") Easiest to stamp precisely
Stainless Steel ±0.06 mm (±0.0025") ±0.08 mm (±0.003") Harder to pierce cleanly; more tool wear
Aluminum ±0.05 mm (±0.002") ±0.10 mm (±0.004") Soft; prone to burring
High-Strength Alloys ±0.08 mm (±0.003") ±0.15 mm (±0.006") Significant springback; needs robust tooling

The Datum Strategy

One lesson we have learned over hundreds of projects: always tie your key tolerances to functional datums. A functional datum is a formed surface or primary feature that the part physically contacts during assembly. When you reference dimensions from a datum rather than a raw blank edge, your measurements become more repeatable and your inspection results more meaningful. This is a core principle of Geometric Dimensioning and Tolerancing.

Also consider whether to use bilateral or unilateral tolerances. Bilateral (±) works best for centered features like holes and slots. Unilateral (+0/–X or –0/+X) works best when you need to guarantee clearance and avoid interference.

✔ Same-plane pierced features can hold ±0.05 mm in progressive dies True
Progressive die stamping eliminates part re-positioning errors between stations, making hole-to-hole dimensions on the same plane extremely accurate and repeatable.
✘ Formed features can achieve the same tight tolerances as flat pierced features False
Formed features like bends and drawn heights inherently have wider tolerances because material springback, grain direction, and thickness variation all compound during forming operations.

Can Tighter Tolerances Increase My Stamping Costs and Lead Times?

The short answer is yes — and the increase is not linear, it is exponential. We worked with a client who wanted ±0.05 mm on every bend height across a complex multi-planar bracket. The quoting exercise from three different die shops came back with prices 50–70% higher than the same part at ±0.2 mm on non-critical bends. The inspection overhead alone doubled.

Tighter tolerances significantly increase stamping costs and lead times. Moving from ISO 2768-m to ISO 2768 Fine can raise tooling costs by 30–60%, increase inspection frequency, and drive up scrap rates. The cost escalation comes from precision die construction, tighter quality control standards, more frequent tooling wear compensation, and higher rejection rates.

Tighter tolerances raise stamping costs, tooling expenses, and lead times

Where the Extra Cost Comes From

There are four main cost drivers when you tighten tolerances beyond standard capability:

1. Tooling complexity. A die that holds ±0.05 mm on formed features needs tighter clearances, hardened inserts, and more stations in a progressive die. Single-stage dies may need to become compound or progressive dies. This alone can add thousands of dollars to your tooling investment.

2. Inspection overhead. Standard stamping parts might need first-article inspection and periodic checks every few thousand pieces. Tight-tolerance parts often require 100% inspection on critical dimensions, CMM verification, or even in-die piezo sensors for real-time dimensional verification. This emerging "Smart Tooling" technology is powerful but adds cost.

3. Scrap rate. As tolerances tighten, the window for acceptable parts shrinks. Normal process variation — from material batch differences, press speed, lubrication, and tooling wear compensation cycles — pushes more parts outside the acceptance window. Higher scrap means higher unit cost.

4. Lead time. Precision dies take longer to build. They also require more tryout runs and fine-tuning. And when something drifts during production, rework and adjustment cycles extend delivery schedules. This is a real pain point for buyers who need on-time delivery.

The Springback Factor

Material springback is the single biggest enemy of tight tolerances on formed features. When a punch bends sheet metal, the metal tries to spring back toward its original shape. The amount of springback depends on the material type 5, sheet metal thickness, bend radius, and grain direction relative to the bend line. Toolmakers use over-bending and anisotropic compensation to fight springback, but these techniques have limits.

Burr Height: A Hidden Tolerance

Standard tolerance grades do not include burr height 6 specifications. Yet burr height directly affects the functional envelope of a part. A general rule is that burr should not exceed 10% of material thickness. If your part goes through electroplating afterward, remember that plating can add 5–15 microns. This means a part that passes "pre-plate" inspection might fail "post-plate" if the tolerance was already at the edge. Always clarify on your drawing whether dimensions apply before or after surface treatment.

When Tighter Is Worth It

Not all tight tolerances are wasteful. For electrical contacts, sensor housings, or parts that must mate with zero play, investing in precision stamping at ±0.05 mm is justified. The key is to apply tight tolerances selectively — only to the features that demand them — and let everything else sit at ISO 2768-m or ST3–ST5.

How Can I Ensure My Supplier Consistently Meets the Tolerance Grades Specified on My Drawings?

A few years ago, we onboarded a new stamping supplier in Vietnam for a U.S. client's automotive bracket program. The first samples were perfect. By the fifth production run, three dimensions had drifted out of spec. The root cause was tooling wear — the die had stamped 200,000 parts without a sharpening cycle. That experience reshaped how we manage supplier quality.

To ensure your supplier consistently meets tolerance grades, require a PPAP (Production Part Approval Process) at launch, establish clear inspection frequency plans, demand SPC data on critical dimensions, audit the supplier's tooling maintenance schedule, and specify burr height and plating-related dimensional requirements explicitly on your drawings.

Ensuring supplier compliance with tolerance grades via PPAP and SPC data

Start with a Complete Drawing

The most common reason suppliers deliver non-conforming stamped parts is not poor capability — it is incomplete drawings. Our China engineering team has reviewed hundreds of customer drawings, and these are the items most frequently missing:

  • General tolerance class (e.g., "ISO 2768-m" or "per DIN 6930-f")
  • Datum references for critical dimensions
  • Burr direction and maximum burr height
  • Whether dimensions are pre-plate or post-plate
  • Surface finish requirements on specific faces

If your drawing does not state a general tolerance class, the supplier will assume one. Their assumption may not match yours. Always call out the standard explicitly in the title block.

Use PPAP to Lock In Capability

PPAP — Production Part Approval Process 7 — is the gold standard for validating that a supplier can consistently produce parts within tolerance. At our company, we manage the full PPAP process for our U.S. clients. This includes dimensional reports on multiple samples, capability studies (Cpk) on critical features, material certifications, and control plans.

A Cpk of 1.33 8 or higher on critical dimensions means the process is centered and capable. If a supplier cannot demonstrate this at PPAP, they will struggle in mass production.

Monitor Tooling Wear

Stamping dies wear over time. Punches dull. Die clearances open up. This is normal, but it must be managed. The best suppliers track cumulative shot counts and schedule preventive maintenance — sharpening, insert replacement, and alignment checks — at defined intervals. We audit this as part of our supplier management process.

Tooling wear compensation is not a one-time calibration. It is an ongoing discipline. Ask your supplier for their maintenance log and correlate it with SPC data. If you see dimensional drift correlating with high shot counts, the maintenance interval needs to be shortened.

Leverage In-Process Inspection

Final inspection catches defects. In-process inspection prevents them. Progressive die stamping is well-suited to in-die sensing. Modern "Smart Tooling" uses piezo sensors embedded in the die to measure force profiles on every stroke. An abnormal force signature — caused by a worn punch, a material anomaly, or a misaligned strip — triggers an alarm before hundreds of bad parts are stamped.

Even without in-die sensors, a good supplier performs periodic dimensional checks 9 during the run. For standard parts, this might be every 500–1,000 pieces. For tight-tolerance parts, it might be every 100 pieces or even continuous monitoring.

Communicate Clearly Across Borders

When sourcing stamping parts internationally, standard names differ. A buyer writing "ISO 2768-m" on a drawing sent to a Chinese supplier who works in GB/T13914 needs to ensure the supplier maps the tolerance correctly. At our offices in China and Vietnam, our engineers bridge this gap daily. We translate tolerance requirements between ISO, DIN, ASME Y14.5 10, and GB standards so nothing is lost in translation.

This cross-border translation is one of the most overlooked risks in international sourcing. If your supplier misinterprets "Fine" as their local "Medium," you will not discover the problem until parts arrive — and by then, tooling is cut and production has run. To minimize such risks, it's essential to define quality standards and acceptance criteria for stamping parts contracts before production begins.

✔ PPAP with Cpk data is the most reliable way to validate a stamping supplier’s tolerance capability True
PPAP requires statistical evidence (Cpk ≥ 1.33) that the process is centered and capable, providing objective proof that the supplier can hold the specified tolerance grade consistently across production runs.
✘ If the first sample passes inspection, the supplier will hold tolerance for the entire production run False
Tooling wear, material batch variation, and press condition changes cause dimensional drift over time. Without ongoing SPC monitoring and preventive die maintenance, tolerances will eventually shift out of spec.

Conclusion

Understanding tolerance grades for stamping parts — from ST/FT systems to ISO 2768-m and DIN 6930-f — lets you specify only what you need and avoid costly over-tolerancing. For further guidance on setting stamping part tolerances for assembly compatibility, explore how to align your tolerance specifications with real-world assembly requirements.


Frequently Asked Questions

What Are the Standard Tolerance Grades Used in Metal Stamping and How Do They Affect My Sourcing Decisions?

A purchasing manager in Ohio once sent us a drawing with every dimension marked "Fine." When our engineering team in China reviewed it, we found that only three of the twenty-two dimensions actually needed that level of dimensional accuracy. The rest could safely sit at "Medium."

How Do I Know Which Tolerance Grade Is Right for My Custom Stamped Parts?

Last quarter, we ran a DFM review for a client whose bracket had twelve holes. Only two holes were alignment-critical. The rest were clearance holes for M4 screws. We recommended ±0.05 mm for the two critical holes and ±0.2 mm for everything else. That single change cut their die cost by roughly 15%.

Can Tighter Tolerances Increase My Stamping Costs and Lead Times?

The short answer is yes — and the increase is not linear, it is exponential. We worked with a client who wanted ±0.05 mm on every bend height across a complex multi-planar bracket. The quoting exercise from three different die shops came back with prices 50–70% higher than the same part at ±0.2 mm on non-critical bends. The inspection overhead alone doubled.

Footnotes


1. Overview of the international standard for general tolerances in technical drawings. ↩︎


2. Technical resource on the requirements and manufacturing of automotive structural components. ↩︎


3. Official source for the DIN 6930-2 standard governing tolerances for stamped steel parts. ↩︎


4. The definitive standard for GD&T, ensuring clear communication of engineering tolerances. ↩︎


5. Scientific resource explaining how material properties influence manufacturing outcomes. ↩︎


6. Engineering reference defining burr formation and its impact on part quality. ↩︎


7. Comprehensive overview of the standard automotive quality assurance process. ↩︎


8. Official government handbook explaining process capability indices like Cpk for quality control. ↩︎


9. Provides guidance on establishing quality control plans and inspection routines in manufacturing. ↩︎


10. Detailed explanation of the ASME Y14.5 standard for dimensioning and tolerancing. ↩︎

Manufacturing RFQ

Have a STEP Model or 2D Drawing for This Project?

Share your drawing, material, quantity and finishing requirements to begin a manufacturing quote. Confirm pricing, delivery and inspection requirements during the review.

Upload CAD & Get Quote →

This article is part of DEWIN's technical manufacturing engineering knowledge base. Factory-specific details come from each factory's profile page — please verify current information there or with our team.

Quick Sourcing Inquiry